ASTM-D4781:2008 Edition(Redline)
$23.40
D4781-03(2008) Standard Test Method for Mechanically Tapped Packing Density of Fine Catalyst Particles and Catalyst Carrier Particles (Redline)
Published By | Publication Date | Number of Pages |
ASTM | 2008 | 3 |
This test method is for measuring the mechanically tapped packing density of powders that are smaller than 0.8 mm in diameter, such as Fluidized Catalytic Cracking Catalysts (FCC).
1. Scope
1.1 This test method covers the determination of the mechanically tapped packing density of fine catalyst and catalyst carrier particles smaller than 0.8 mm in diameter.
1.2 This standard does not purport to address all of the safety concerns, if any associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
2. Referenced Documents (purchase separately) The documents listed below are referenced within the subject standard but are not provided as part of the standard.
ASTM Standards
D3766 Terminology Relating to Catalysts and Catalysis E177 Practice for Use of the Terms Precision and Bias in ASTM Test Methods E456 Terminology Relating to Quality and Statistics E691 Practice for Conducting an Interlaboratory Study to Determine the Precision of a Test Method
Keyword