Shopping Cart

No products in the cart.

ASTM-E140:2002 Edition

$58.50

E140-02 Standard Hardness Conversion Tables for Metals Relationship Among Brinell Hardness, Vickers Hardness, Rockwell Hardness, Superficial Hardness, Knoop Hardness, and Scleroscope Hardness

Published By Publication Date Number of Pages
ASTM 2002 21
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

1.1 Conversion presents data in the Rockwell C hardness range on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, Rockwell superficial hardness, Knoop hardness, and Scleroscope hardness of non-austenitic steels including carbon, alloy, and tool steels in the as-forged, annealed, normalized, and quenched and tempered conditions provided that they are homogeneous.

1.2 Conversion Table 2 presents data in the Rockwell B hardness range on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, Rockwell superficial hardness, Knoop hardness, and Scleroscope hardness of non-austenitic steels including carbon, alloy, and tool steels in the as-forged, annealed, normalized, and quenched and tempered conditions provided that they are homogeneous.

1.3 Conversion Table 3 presents data on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, Rockwell superficial hardness, and Knoop hardness of nickel and high-nickel alloys (nickel content over 50 %). These hardness conversion relationships are intended to apply particularly to the following: nickel-aluminum-silicon specimens finished to commercial mill standards for hardness testing, covering the entire range of these alloys from their annealed to their heavily cold-worked or age-hardened conditions, including their intermediate conditions.

1.4 Conversion Table 4 presents data on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, and Rockwell superficial hardness of cartridge brass.

1.5 Conversion Table 5 presents data on the relationship between Brinell hardness and Rockwell B hardness of austenitic stainless steel plate in the annealed condition.

1.6 Conversion Table 6 presents data on the relationship between Rockwell hardness and Rockwell superficial hardness of austenitic stainless steel sheet.

1.7 Conversion Table 7 presents data on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, Rockwell superficial hardness, and Knoop hardness of copper.

1.8 Conversion Table 8 presents data on the relationship among Brinell hardness, Rockwell hardness, and Vickers hardness of alloyed white iron.

1.9 Conversion Table 9 presents data on the relationship among Brinell hardness, Vickers hardness, Rockwell hardness, and Rockwell superficial hardness of wrought aluminum products.

1.10 Many of the conversion values presented herein were obtained from computer-generated curves of actual test data. Most Rockwell hardness numbers are presented to the nearest 0.1 or 0.5 hardness number to permit accurate reproduction of these curves. Since all converted hardness values must be considered approximate, however, all converted Rockwell hardness numbers shall be rounded to the nearest whole number in accordance with Practice E 29.

1.11 Appendix X1-Appendix X9 contain equations developed from the data in Tables 1-9, respectively, to convert from one hardness scale to another. Since all converted hardness values must be considered approximate, however, all converted hardness numbers shall be rounded in accordance with Practice E 29.

1.12 Conversion of hardness values should be used only when it is impossible to test the material under the conditions specified, and when conversion is made it should be done with discretion and under controlled conditions. Each type of hardness test is subject to certain errors, but if precautions are carefully observed, the reliability of hardness readings made on instruments of the indentation type will be found comparable. Differences in sensitivity within the range of a given hardness scale (for example, Rockwell B) may be greater than between two different scales or types of instruments. The conversion values, whether from the tables or calculated from the equations, are only approximate and may be inaccurate for specific application.

PDF Catalog

PDF Pages PDF Title
1 Scope
Referenced Documents
2 Methods for Hardness Determinations
Apparatus and Reference Standards
Principle of Method of Conversion

Significance and Use
Reporting of Hardness Numbers
Keywords

3 TABLE 1
4 TABLE 2
6 TABLE 3
9 TABLE 4
11 TABLE 5
12 TABLE 6
14 TABLE 7
15 TABLE 8
TABLE 9
16 X1. HARDNESS CONVERSION EQUATIONS FOR NON-AUSTENITIC STEELS (DETERMINED HARDNESS SCALE NUMBERS TO ROCKWELL C HARDNESS NUMBERS)
X1.1
X2. HARDNESS CONVERSION EQUATIONS FOR NON-AUSTENITIC STEELS (DETERMINED HARDNESS SCALE NUMBERS TO ROCKWELL B HARDNESS NUMBERS)
X2.1
17 X3. HARDNESS CONVERSION EQUATIONS FOR NICKEL AND HIGH-NICKEL ALLOYS (DETERMINED HARDNESS SCALE NUMBERS TO VICKERS HARDNESS NUMBERS)
X3.1
18 X4. HARDNESS CONVERSION EQUATIONS FOR CARTRIDGE BRASS (DETERMINED HARDNESS SCALE NUMBERS TO VICKERS HARDNESS NUMBERS)
X4.1
X5. HARDNESS CONVERSION EQUATION FOR ANNEALED AUSTENITIC STAINLESS STEEL PLATE (DETERMINED BRINELL HARDNESS NUMBERS TO ROCKWELL B HARDNESS NUMBERS)
X5.1
X6. HARDNESS CONVERSION EQUATIONS FOR AUSTENITIC STAINLESS STEEL SHEET (DETERMINED HARDNESS SCALE NUMBERS TO ROCKWELL C OR ROCKWELL B HARDNESS NUMBERS
X6.1
19 X7. HARDNESS CONVERSION EQUATIONS FOR COPPER, NOS. 102 TO 142 INCLUSIVE (DETERMINED HARDNESS SCALE NUMBERS TO VICKERS HARDNESS NUMBERS)
X7.1
20 X8. HARDNESS CONVERSION EQUATIONS FOR ALLOYED WHITE IRON (DETERMINED HARDNESS SCALE NUMBERS TO VICKERS HARDNESS NUMBERS)
X8.1
X9. HARDNESS CONVERSION EQUATIONS FOR WROUGHT ALUMINUM PRODUCTS (DETERMINED HARDNESS SCALE NUMBERS TO BRINELL HARDNESS NUMBERS)
X9.1
X10. EFFECT OF STRAIN HARDENING ON HARDNESS CONVERSION RELATIONSHIPS
X10.1
X10.2
ASTM-E140